Electroplated zinc and zinc-nickel are common finishes on made-to-print fasteners and related components. They are different systems, and each may be specified with a particular chromate, passivate or seal, a thickness range, and an appearance or friction condition. Those details are taken from the current revision and from any referenced specification. A colour sample, a “silver zinc” shop shorthand, or a flake finish that happens to look similar is not a substitute for the named electroplated system.
What has to be visible on the revision
A complete call-out names the system (zinc or zinc-nickel, and any alloy range if the specification uses one), the thickness or the performance class, the chromate or seal, and any appearance, lubrication or friction requirement. “Zinc plate, yellow” or “Zn-Ni, black” without a specification is not complete, because colour is not the system. If a customer or industry standard already defines the deposit and the after-treatment, it should be named on the revision or attached to the enquiry.
Thread class and post-coat gauging have to be consistent with the deposit thickness, as in the note on coating thickness and thread class. Friction modifiers and supplementary lubricants, when they are specified, stay with the finish, as in the note on friction class and torque-tension. Process steps that belong with high-strength electroplated parts, including any required relief of hydrogen embrittlement, are covered in the existing note on coatings for high-strength fasteners and are not repeated here.
Electroplated zinc and zinc-nickel are not interchangeable
The two deposits do not have the same thickness-to-performance relationship, the same appearance range, or the same behaviour with seals and topcoats. A sample in electroplated zinc is not approval of a later zinc-nickel route, or the reverse, when the print names one of them. A change of chromate or seal, or a change from a clear to a black after-treatment, is likewise a process change if the specification names that after-treatment. Those changes are re-validated before serial release, not decided from a colour chip after the first coated lot.
Inspection follows the specification
Thickness, appearance, adhesion, or a salt-spray requirement are used when the print or the order requires that evidence, not automatically in every possible form. If a particular thickness location, a first-article coated layout, or a named test is already decided, name it. A visual match to a previous lot, or a photograph of a yellow or black finish, is not a substitute for the system and the thickness written on the print. Certificates and any EN 10204 3.1 evidence are confirmed per order when required. Neutral salt-spray hours, when they appear, follow the specification and are not published here as a site result.
Open items and conflicts
A print that names zinc in one note and zinc-nickel in another, or that asks for a flake system and an electroplated system as if they were alternatives without a stated choice, is flagged. An IMDS entry, when required, has to follow the deposit and the after-treatment that are actually used.
Rack, barrel and mixed routes are not silent alternatives
Electroplated fasteners may be racked or barrel-plated, and the two routes do not leave the same thickness distribution on heads, shanks and threads. That choice is a process decision and is stated rather than assumed. A racked sample is not automatic approval of a later barrel route, or the reverse, when thickness, appearance or post-coat gauging is specified. Recesses and internal threads need particular attention, as in the note on coating on internal threads.
Volume and the proposed plating route also belong in the enquiry. A change of deposit, of chromate or seal, or of rack versus barrel after samples have been approved is a process change and is re-validated before serial release. First-article inspection, when required, should be planned on the production-intent coating route, as in the note on first-article inspection. The current drawing revision remains the source of the electroplating requirement in every case.
The enquiry should also identify any requirement for a particular alloy range in the zinc-nickel deposit, for a minimum or maximum after-treatment film, or for a ban on hexavalent chromium if those notes already exist in the customer specification. They are reviewed as written. A colour word such as black or yellow is additional appearance information; it is not the deposit name, as in the note that colour is not the coating system. If first-article inspection must include thickness maps on heads, shanks and threads, that should be stated so that the production-intent rack or barrel route can be planned around it.
Storage, handling and later assembly can also scuff a chromate or a seal. If the specification limits handling marks, packing belongs in the agreed route, as in the note on packing, labelling and lot traceability. A change of after-treatment to “hide” marks is still a specification change. Thickness, appearance and post-coat gauging remain as written on the current revision, not as improved after the fact in the stores.
What to send with the RFQ
Send the current drawing revision, the coating specification, and any standard that defines the deposit, the after-treatment and the gauging condition. If post-coat gauging, a friction class or a particular appearance is already required, say so. Volume belongs in the enquiry. Unspecified points will be flagged before production rather than assumed.
This article is a capability and commercial note. It is not a certificate, a dimensional data book, or evidence of customer approval. Catalogue type codes and example grades do not replace the customer’s item number, material specification or drawing revision.